PASSAWARNPASSAWARNConsult on LINE

Method · Cementitious waterproofing

Two coats, brushed on.

Cement powder mixed with a liquid polymer and brushed or trowelled on in two coats. The polymer lets it follow small movement — for water tanks, pools and basements.

What it is

What it is

Cement powder mixed with a liquid polymer, brushed or trowelled on as a thin coat. The polymer gives it enough flexibility to follow small movement.

Choose it when

Water tanks, pools and basements — a potable-water grade is available for tanks that hold drinking water.

Keep in mind

Applied in two coats on a damp surface with no standing water; the tank is filled for the water-holding test only after the cure time in the product's data sheet (usually several days).

How it is built

Layers (built up from the bottom)

  1. Cementitious waterproofing, coat 2

    Applied once the first coat has set, to build an even thickness.

  2. Cementitious waterproofing, coat 1

    Applied to the damp substrate. It bonds with the concrete to stop water.

  3. Concrete (pre-dampened)substrate

    Soaked with water, surface left just dry, so it won’t draw water out of the coating.

The figure shows one typical build-up. The actual layers are decided after we see the site.

How we install & check

Two-coat cementitious

Applied in two coats on a damp surface with no standing water; the tank is filled for the water-holding test only after the cure time in the product's data sheet (usually several days).

Prove it holds water

Roofs and tanks get a water (ponding) test before handover; the result is signed off jointly.

Other cementitious systems, by use

Cementitious systems are chosen by whether the concrete is new or existing, and where it is. If another one fits better, we will say so.

SystemStrengthWhere
Surface Apply — Polymer Modified (A+B)this pageFollows substrate movement, resists crackingWater tank, pool, below ground
Surface Apply — Rigid Slurry (1-part)Low-cost, but weak to crackingSimple, low-budget
CrystallizationCrystals grow in the pores and close fine, non-moving cracksBelow ground, foundation, tunnel
Integral AdmixtureMakes the concrete itself watertight — joints treated separatelyNew waterproof concrete
Active Leak Plugging (Water Plug)Plugs a running leak in minutesEmergency leak stop

Projects

Also with this method:MRT Orange Line

Common problem

Questions

What decides the price?

The area, the state of the substrate (cracks, wet spots, or an old membrane to remove), the system and number of layers, whether it is exposed to the sun, and the hours we can work. Send photos and drawings on LINE and we will check the site and quote.

Can it be used in drinking-water tanks?

Yes — a potable-water grade is available for tanks that hold drinking water.

When can the tank be filled?

It is applied in two coats on a damp surface. The tank is filled for the water-holding test only after the cure time in the product's data sheet — usually several days (about 3 to 14) — which we confirm first.

By industry

Tell us about the structure.

Send the drawings, what the structure holds and when it will be poured. We propose the system that fits.

Only want materials? psw-chemical.com ↗TEL +66 2 552 6468 · sales@passawarn.com